Calcium and magnesium salts in hard water precipitate on surfaces as insoluble carbonate and sulphate layers when heated or evaporated. A scale layer acts like thermal insulation: even a thin layer significantly reduces heat transfer efficiency, increases energy consumption, narrows the flow cross-section and creates conditions for under-deposit corrosion.
Where scale problems occur
- Plate and shell-and-tube heat exchangers,
- Steam and hot water boilers,
- Cooling towers and closed-loop cooling systems,
- Cooling channels of plastic injection and die-casting moulds,
- Compressor and hydraulic unit coolers, industrial dishwashers and washing machines.
The type of scale matters
| Layer | Characteristics | Cleaning approach |
|---|---|---|
| Calcium carbonate | The most common type of scale, sensitive to acid | Easily dissolved with an acidic descaler |
| Calcium sulphate (gypsum) | Dissolves poorly in acid | Products designed for this layer, longer contact time |
| Silicate layers | Very hard, glass-like | Special product and mechanical support may be needed |
| Iron oxide / rust-mixed layer | Brown, mixed with corrosion products | Products that dissolve rust and scale together |
Choosing a descaler by material
- Carbon steel: Descalers suitable for steel; contact time must be controlled.
- Stainless steel: Choose products suitable for stainless steel; unsuitable products increase the risk of pitting corrosion.
- Copper and brass: Low-aggressiveness products suitable for copper alloys.
- Aluminium and galvanised steel: Use only products suitable for these metals.
Circulation (CIP) descaling steps
- Take the system out of service and drain the water.
- Connect a circulation pump: The descaler is circulated through the system via a tank.
- Add the descaler: Carbon dioxide released during dissolution can create foam and pressure. The system must be vented.
- Monitor the pH: If the pH rises, the acid has been consumed; top up until the scale is completely dissolved.
- Drain and rinse: Rinse with clean water until the pH is neutral.
- Neutralisation and passivation: If necessary, apply mild alkaline neutralisation and a rust inhibitor.
- Waste management: The spent solution is neutralised and disposed of in accordance with regulations.
Preventing scale from forming again
- Improving feed water by softening or reverse osmosis,
- Using a suitable water conditioner in cooling water,
- Periodic maintenance and monitoring of temperature difference (ΔT); a drop in heat transfer is an early sign of scaling.
Frequently asked questions
Can a plate heat exchanger be cleaned without dismantling?
Yes. A heat exchanger can be cleaned without dismantling using the circulation (CIP) method. In cases of very heavy blockage, the plates may need to be removed and cleaned by immersion.
Is it right to use raw acid for descaling?
Raw acids can severely corrode metal and cause corrosion on stainless steel. For equipment cleaning, descalers developed for the specific material should be used.
How often should descaling be done?
It depends on water hardness, operating temperature and intensity of use. The best approach is to set the interval by monitoring heat transfer performance and pressure drop.
Support for your descaling application
Molkim offers descaling chemicals for carbon steel, stainless steel and copper alloys. If you share the equipment type, material and type of scale, we can determine the right product and application method together.
Related products: Descaling Chemicals · Rust Removal Chemicals · Contact