Cutting fluids used in CNC turning and milling leave an oil film, fine chips and metal dust on parts. On parts that undergo heat treatment, welding or high-temperature operation, oils carbonise into a burnt, black and hard residue. These residues cause serious problems for assembly, measurement, coating and sealing.
Types of contamination
| Contamination | Characteristics | Cleaning approach |
|---|---|---|
| Neat cutting oil | Mineral-based, thick film | Emulsifying alkaline cleaner or solvent |
| Soluble oil (water-based emulsion) | Sticky when dry, can leave salt and soap residue | Alkaline cleaner, good rinsing |
| Synthetic / semi-synthetic coolants | Polar; rinse off easily with water but can leave residue | Mild alkaline or neutral cleaner |
| Chips and metal dust | Accumulate in blind holes and threads | Mechanical support with ultrasonics and spray, filtration |
| Carbonised, burnt oil | Hard, black, adhered to the surface | Strong alkaline, high temperature, long time and ultrasonics |
Recommended cleaning sequence
- Chip removal: Coarse chips are removed by air blowing or pre-rinsing.
- Degreasing: Alkaline ultrasonic or spray washing. On lines with a high oil load, oil-splitting (demulsifying) cleaners extend bath life.
- Rinsing: At least one stage, two for critical parts.
- Rust protection: Adding a water-based rust inhibitor to the rinse water for steel parts.
- Drying: Hot air or vacuum drying; vacuum drying is recommended for blind holes.
Special approach for carbonised residues
- Pre-soak: Parts are soaked for a long time in a strong alkaline bath to soften the residue.
- High temperature: The effectiveness of the chemical increases significantly with temperature.
- Ultrasonic support: Lifts the softened residue from the surface.
- Material compatibility: Products suitable for aluminium and non-ferrous metals must be used on these materials.
Technical cleanliness and particle control
In the automotive and hydraulics sectors, parts are inspected for particulate contamination according to standards such as VDA 19 and ISO 16232. For cleanliness at this level, filtration, rinse stages and a clean drying environment must be planned in addition to the right chemical.
Frequently asked questions
Why does soluble oil residue leave white stains?
Salts and additives in the soluble oil emulsion leave white stains on the surface when the water evaporates. They are removed with alkaline cleaning and adequate rinsing.
Blasting or chemicals for burnt oil residue?
Blasting can affect dimensions and surface quality and cannot reach blind holes and internal channels. Chemical and ultrasonic cleaning provides uniform cleaning of complex geometries without affecting dimensions.
Support for machining cleaning
Molkim offers ultrasonic, immersion and spray washing chemicals for cutting oil, soluble oil and carbonised residues. If you share your part material, the cutting fluid used and your cleaning requirements, we can determine the right solution together.
Related products: Ultrasonic and Immersion Bath Chemicals · Degreasing Chemicals · Cleaning Chemicals for Ultrasonic and Spray Washing Machines · Contact