After machining, pressing, rolling and heat treatment, machining oils, cutting fluids, rust-preventive films and greases remain on the surface of metal parts. If painting, phosphating, galvanising, PVD or welding is carried out without removing these contaminants, adhesion failures, blistering, porosity and colour variations appear. Degreasing is the first and most critical step of the entire surface treatment chain.
Degreasing methods
- Immersion: Parts are immersed in a heated alkaline bath. Efficiency increases with movement, air agitation or ultrasonic support.
- Ultrasonic: The most effective method for blind holes, threads and complex geometries.
- Spray washing: Soil is removed by mechanical pressure; requires special low-foam products.
- Solvent degreasing: Applied in closed solvent machines for water-sensitive parts and very short cycle times.
- Electrolytic degreasing: As a final activation step in plating lines; gas bubbles generated under current clean the surface at micro level.
Emulsifying and demulsifying cleaners
How alkaline degreasing chemicals behave with oil in the bath directly determines bath life and waste cost.
| Emulsifying | Demulsifying (oil-splitting) | |
|---|---|---|
| Behaviour of the oil | Oil stays in the bath as an emulsion | Oil rises to the bath surface |
| Advantage | Oil does not redeposit; very clean surface at low oil load | Removed with a skimmer or separator, bath life is extended |
| Disadvantage | When oil accumulates the whole bath must be replaced | Skimming equipment needed; parts must not pick up oil on exit |
| Best suited for | Low oil load, critical cleaning | High oil load, continuous lines |
Process control
- Concentration: Measure regularly by titration (free and total alkalinity) and top up the consumed chemical.
- Temperature: Most alkaline degreasing works at 50–80 °C; low-temperature products save energy.
- Oil load: Cleaning quality drops as the oil content of the bath rises; oil separation and bath change intervals should be defined.
- Rinsing: At least two rinse stages prevent alkali being carried into the next bath (drag-out).
How to verify degreasing quality
- Water break test: The water film on a part leaving the rinse must remain continuous.
- White cloth or paper test: Residue check by wiping.
- Test ink (dyne): Surface energy check before painting and bonding.
- Gravimetric method and particle analysis: Measurement of residue quantity in technical cleanliness specifications.
Frequently asked questions
Why do parts rust after degreasing?
Alkaline degreasing also removes the protective oil film from the surface. If the part stays wet after rinsing, carbon steel rusts quickly. Prompt drying or the use of a rust inhibitor in the rinse is recommended.
How should aluminium parts be degreased?
Aluminium is etched and dulled in strong alkali. Low-to-medium alkaline products suitable for aluminium should be used, with temperature and time under control.
When should the bath be replaced?
The bath should be replaced if cleaning quality drops even though the concentration has been topped up, if foam and sludge increase, or if the oil load exceeds the defined limit. Regular sample monitoring is recommended to set this limit.
Support for your degreasing process
Molkim offers emulsifying and demulsifying alkaline cleaners and solvent-based solutions for immersion, ultrasonic, spray and electrolytic degreasing. If you share your part material, oil type and current line, we can determine the right product and process parameters together.
Related products: Degreasing Chemicals · Ultrasonic and Immersion Bath Chemicals · Solvent Cleaning Products · Contact